4186. Custom Hastelloy C22 Wire Supplier Short Lead Time with ASTM B574 Standard
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
4187. Custom Hastelloy C22 Wire Supplier Short Lead Time with ASTM B574 Standard
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
4188. Custom Hastelloy C22 Wire Supplier Short Lead Time with ASTM B574 Standard
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
4189. Hastelloy C276 Cold-Drawn Wire Excellent Dimensional Accuracy Smooth Surface for Spring Coiling
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
4190. Precision Drawn Hastelloy C276 C22 B2 Wire, Custom Diameter for Springs Fasteners
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
4191. Precision Drawn Hastelloy C276 C22 B2 Wire, Custom Diameter for Springs Fasteners
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
4192. Spring Temper Hastelloy C276 C22 Wire High Tensile Strength for Precision Fasteners
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
4193. Spring Temper Hastelloy C276 C22 Wire High Tensile Strength for Precision Fasteners
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
4194. Spring Temper Hastelloy C276 C22 Wire High Tensile Strength for Precision Fasteners
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
4195. Hastelloy C22 C276 C4 B2 Wire for Petrochemical Furnace Components Oxidation Resistance
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
4196. Hastelloy C22 C276 C4 B2 Wire for Petrochemical Furnace Components Oxidation Resistance
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
4197. Hastelloy C22 C276 C4 B2 Wire for Petrochemical Furnace Components Oxidation Resistance
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
4198. Hastelloy C22 C276 C4 B2 Wire for Petrochemical Furnace Components Oxidation Resistance
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
4199. Hastelloy C22 C276 C4 B2 Wire for Petrochemical Furnace Components Oxidation Resistance
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
4200. Hastelloy C22 C276 C4 B2 Wire for Petrochemical Furnace Components Oxidation Resistance
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...