Jiangsu Profile

Product List
35581. Quick-Cure UV Glass Coating for High-Speed Production
[Sep 09, 2025]
[Sep 09, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35582. Metallic Effect Glass Paint for Luxury Gift Packaging
[Sep 09, 2025]
[Sep 09, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35583. Glow-in-Dark Water-Based Enamel for Safety Signage
[Sep 09, 2025]
[Sep 09, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35584. Water-Based Rust Converter for Already Rusted Surfaces
[Sep 08, 2025]
[Sep 08, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35585. Low-Odor Water-Based Anti-Rust Paint for Residential Use
[Sep 08, 2025]
[Sep 08, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35586. Heavy-Duty Water-Based Rust Preventive for Industrial Machinery
[Sep 08, 2025]
[Sep 08, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35587. Fast-Drying Water-Based Anti-Corrosion Coating for DIY Projects
[Sep 08, 2025]
[Sep 08, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35588. Eco-Friendly Water-Based Rust Inhibitor for Indoor Metal Furniture
[Sep 08, 2025]
[Sep 08, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35589. Mold-Resistant Alkyd Coating for Humid Environments
[Aug 26, 2025]
[Aug 26, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35590. Self-Priming Water-Based Alkyd Paint for Rusted Surfaces
[Aug 26, 2025]
[Aug 26, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35591. Water-Reducible Alkyd Coating for Environmental Compliance
[Aug 26, 2025]
[Aug 26, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35592. High-Build Water-Based Alkyd Primer for Industrial Equipment
[Aug 26, 2025]
[Aug 26, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35593. Water-Based Alkyd Anti-Rust Primer for Structural Steel
[Aug 26, 2025]
[Aug 26, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35594. Zinc-Rich Alkyd Primer for Enhanced Cathodic Protection
[Aug 25, 2025]
[Aug 25, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35595. Silicone-Modified Alkyd for High Temperature Surfaces
[Aug 25, 2025]
[Aug 25, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...