Jiangsu Profile

Product List
83026. Precision Drawn Hastelloy C276 C22 B2 Wire, Custom Diameter for Springs Fasteners
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
83027. Spring Temper Hastelloy C276 C22 Wire High Tensile Strength for Precision Fasteners
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
83028. Spring Temper Hastelloy C276 C22 Wire High Tensile Strength for Precision Fasteners
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
83029. Spring Temper Hastelloy C276 C22 Wire High Tensile Strength for Precision Fasteners
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
83030. Hastelloy C22 C276 C4 B2 Wire for Petrochemical Furnace Components Oxidation Resistance
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
83031. Hastelloy C22 C276 C4 B2 Wire for Petrochemical Furnace Components Oxidation Resistance
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
83032. Hastelloy C22 C276 C4 B2 Wire for Petrochemical Furnace Components Oxidation Resistance
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
83033. Hastelloy C22 C276 C4 B2 Wire for Petrochemical Furnace Components Oxidation Resistance
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
83034. Hastelloy C22 C276 C4 B2 Wire for Petrochemical Furnace Components Oxidation Resistance
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
83035. Hastelloy C22 C276 C4 B2 Wire for Petrochemical Furnace Components Oxidation Resistance
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
83036. Hastelloy C276 C22 Coil Spool Wire for Chemical Processing Crevice Corrosion Chloride
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
83037. Hastelloy C276 C22 Coil Spool Wire for Chemical Processing Crevice Corrosion Chloride
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
83038. Hastelloy C276 C22 Coil Spool Wire for Chemical Processing Crevice Corrosion Chloride
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
83039. Hastelloy C276 C22 Coil Spool Wire for Chemical Processing Crevice Corrosion Chloride
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
83040. Hastelloy C276 C22 Coil Spool Wire for Chemical Processing Crevice Corrosion Chloride
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...