35656. Self-Priming Water-Based Alkyd Paint for Rusted Surfaces
[Aug 26, 2025]
[Aug 26, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35657. Water-Reducible Alkyd Coating for Environmental Compliance
[Aug 26, 2025]
[Aug 26, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35658. High-Build Water-Based Alkyd Primer for Industrial Equipment
[Aug 26, 2025]
[Aug 26, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35659. Water-Based Alkyd Anti-Rust Primer for Structural Steel
[Aug 26, 2025]
[Aug 26, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35660. Zinc-Rich Alkyd Primer for Enhanced Cathodic Protection
[Aug 25, 2025]
[Aug 25, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35661. Silicone-Modified Alkyd for High Temperature Surfaces
[Aug 25, 2025]
[Aug 25, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35662. Low-Temperature Cure Alkyd Paint for Winter Applications
[Aug 25, 2025]
[Aug 25, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35663. High-Build Alkyd Primer for Heavy-Duty Industrial Equipment
[Aug 25, 2025]
[Aug 25, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35664. Quick-Dry Alkyd Coating for Maintenance and Repair Projects
[Aug 25, 2025]
[Aug 25, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35665. Alkyd Anti-Rust Primer for Structural Steel in Humid Climates
[Aug 25, 2025]
[Aug 25, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35666. Shape Memory Polyurethane for Impact Resistance
[Aug 22, 2025]
[Aug 22, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35667. Quantum DOT Color Technology Polyurethane for Signage
[Aug 22, 2025]
[Aug 22, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35668. Aerogel-Enhanced Thermal Barrier Polyurethane Coating
[Aug 22, 2025]
[Aug 22, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35669. Bio-Based Acrylic Polyurethane with 50% Renewable Content
[Aug 22, 2025]
[Aug 22, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
35670. Catalytic Infrared Curing Polyurethane for Production Lines
[Aug 22, 2025]
[Aug 22, 2025] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...